Thanks to its high nickel content, Sandvik Sanicro 31HT shows very little tendency to precipitate embrittling phases.
Within the 600-700°C (1110-1290°F) temperature range, an intermetallic phase, gamma prime, Ni
3
(Al, Ti), is precipitated, which reduces the ductility of the alloy. To avoid this precipitation some specifications prescribe maximization of the (Ti + Al) content.
Sandvik supplies a modified version of Sandvik Sanicro 31HT in which chemical composition and heat treatment have been adapted to meet this requirement and give the highest possible creep ductility.
.